FW: [MW:3681] POSITIONS IN overlaying

Dear Mr. Asghariali.

 

From ASME Sec-IX, definition of welding positions, the basics welding positions are:-

 

§     Groove  Weld:-

1.      Flat (1G),

2.      Horizontal(2G)

3.      Vertical(3G)

4.      Overhead(4G)

 

§     Fillet Welds:-

1.      Flat (1F),

2.      Horizontal(2F)

3.      Vertical(3F)

4.      Overhead(4F)

 

Same nomenclature and definitions of groove weld position applies for corrosion resistant and hard facing overlays welds also, except that procedures and performance qualification requires to be done on flat plates or pipes as required. Overlay qualification is different from Sec-IX  normal groove weld qualification.

 

Please see QW-462.5(a) , through,---- to (e), for explanations with diagrams.

 

Hope this would be of help to you.

 

Thanks.

 

Pradip Goswami,P.Eng

Senior Engineer/Specialist(Welding-Metallurgy)

Machine Dynamics & Component Integrity Dept.

Engineering & Training Services Division

ONTARIO POWER GENERATION Inc.

PO Box-2000, RR-55(South)

Nanticoke, Ontario,N0A1L0

Tel:-(519) 587-2201, Ext 3107--in Nanticoke

         (416) 231-4111, Ext 5925--in Kipling,Toronto

Fax: (519) 587-6814

Email-pradip.goswami@opg.com.

  


Date: Tue, 17 Nov 2009 04:46:30 -0800
From: asghariali@rocketmail.com
Subject: [MW:3678] POSITIONS IN overlaying
To:
materials-welding@googlegroups.com

Hi All

are overlaying positions same with groove positions?(according ASME IX)

best regards.



--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchanged in this group are members personnel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...