Skip to main content

[MW:1421] Re: ASME B31.3-2006 Ed. Fig. 328.5.2.c

Dear Friends
 
As per ASME 3.31.3 gap is given at the time of fit-up and offcurse after weding that gap will be less than 1.5 mm because of  shrinkage due to welding heat. the meaning of RT is nothing but radiography test and i think your client might have asked you to perfom Rt to check whether 1.5mm gap has been provided or not
not rejected.

Regards,
 
Jivan Dhamane


--- On Wed, 24/12/08, T. Rizal H. <aatkho@gmail.com> wrote:
From: T. Rizal H. <aatkho@gmail.com>
Subject: [MW:1419] Re: ASME B31.3-2006 Ed. Fig. 328.5.2.c
To: materials-welding@googlegroups.com
Date: Wednesday, 24 December, 2008, 11:35 PM

1.5 mm gap is set before welding, it is to accomodate shrinkage after welding. Of course, gap will be less than 1.5 after welding, but it is not rejected.  What's the meaning after RT?, it is strange to perform RT on the fillet weld.  Regards,  Tex  2008/12/24  <nozhan@cimtas.com.tr>: > > > (Embedded image moved to file: pic14310.jpg) > After welding, less than 1.5 mm gap is the cause to reject the weld after > RT? > If yes, in accordance which criteria? > > Thanks... > > > > Nebi ÖZHAN > > e-mail:nozhan@cimtas.com.tr > > >    --  Regards,  T. Rizal Hidayat   


Unlimited freedom, unlimited storage. Get it now --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...