Skip to main content

[MW:1388] Re: Calibration, Validation of welding machines as per BS 7570 standard.

Dear R.bose,
Refer API 6A for frequency details.
Thanks and Regards,
K.Rajagopal

 
On 12/2/08, Rituraj Bose <boser2006@gmail.com> wrote:

Dear Mr. Muniyandi,

Will you please inform where I can get the details of this frequencies
for calibration?

Regards,
R. Bose

On Dec 1, 12:22 pm, "Muni Andy" <cmkf...@gmail.com> wrote:
> Dear Friends,
> Welding equipments need calibration i e the ammeter and voltmeter is to be
> calibrated.Frequency is once in 3 months.
> validation is required for the welding process and not for welding
> equipments.
> Regrds,
> C.Muniyandi
>
>
>
> On Mon, Dec 1, 2008 at 11:43 AM, <kata...@bilfal.com> wrote:
>
> > Dear friends,
>
> > I am not very clear about the words Calibration, Validation of welding
> > equipments.
>
> > Calibration is defined in some of the literature as all the operations for
> > the purpose of determining the value or errors of a measuring instruments.
> > (Checking the measuring instruments correctness such as A, V meters)
>
> > where as Validation is defined as all the operations for the purpose of
> > demonstrating that an item of Arc welding equipment or welding system
> > complies with the operating specification for that welding equipment or
> > syestem( Checking the correctness of equipment).
>
> > I seen many fabrication  shops  doing calibration not Validation.
>
> > BS 7575-2000  is also having titile  " Code of Practice for Validation of
> > arc welding equipment".
>
> > Can any body  suggest me  wether welding equipment requires  Calibraion or
> > Validation?
>
> > Regards
>
> > P.K- Hide quoted text -
>
> - Show quoted text -
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...