Thursday, August 28, 2008

[MW:1073] The influence of flux TiO2, MnO and Al2O3 for welding properties

Dear Members

I have a problem with my reseach, i want to know the influence of
those flux ability to change the properties of weld metal. Know i was
found an advantage that flux TiO2 can increase the mechanical
properties of weld metal. from the AWS Standard they say that E6013
will have 430-460 MPa of minimum strength, but i had 508 MPa with
E6013 by adding flux TiO2 in electrode face.

My analysis now just from the mechanical test, i was find an acicular
ferrite structure in this research. But i don't know how the
accicular ferrite function for the mechanical properties of weld metal
and the theory of the influence of flux TiO2, MnO and Al2O3
accurately.

I need yours help for all members that want to partcipate.

thanks so much...

note : this research done in Mechanical Engineering Departmet,
University of Andalas, West Sumatra, Indonesia.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...