hai friends
is there any thumb rule to find current and voltage in metal active
gas welding ... v r using semi automatic MAG machine.with 2.4 mm
filler wire dia .current in the rang of 570-670 amps and voltage
30-39 .and tell wat would b the best way to reduce spattesrs and blow
holes and cracks in this welding .

--~--~---------~--~----~------------~-------~--~----~