[MW:1018] CS or LTCS material as per STOOMWEZEN Rules ( PED rules ) - Dutch Power piping code

Hello All,

Can anyone explain me about the Impact test requirement of material as
per Stoomwezen rules ?
from ASME 31.3 we can find the Impact test requirement for CS, as per
thickness and minimum design temperature.
But in Stoomwezen rules there is a minimum requirement of rupture
energy of 27 J.
I have to design a pipe class with -20 deg C as minimum temperature
for 145 bar pressure and size of 30 inch & carrosion allowance of 6 mm
With these design condition I expect to have very high thickness for
pipe.
is it possible to have cofirm 27 J requirement for such high thickness
of CS ?
Or it is advisable to change to LTCS material ?

thank you,

RahuL P

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...