Thursday, August 7, 2008

[MW:1004] RE: 1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503 -224 -GR. 28

Why don't you check in EN 10222 for the required grade? As BS 1503 is
obsolete, no use of searching for similar of equivalent grades.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of shailesh dave
Sent: Thursday, August 07, 2008 3:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:1002] Re: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503
-224 -GR. 28


YES IT IS FORGING MATERIAL.

REGARDS,

S.N.DAVE


--- On Thu, 8/7/08, Bathula Raghuram (Mumbai - PIPING)
<R.Bathula@ticb.com> wrote:

> From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
> Subject: [MW:1000] RE: 999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503
-224 - GR. 28
> To: materials-welding@googlegroups.com
> Date: Thursday, August 7, 2008, 3:22 PM
> Is it a forging material? BS1503 is superseded and replaced
> by EN 10222,
> please check?
>
> ________________________________
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of
> shailesh dave
> Sent: Thursday, August 07, 2008 2:28 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:999] Re: 993] EQUVIVALENT ASME GRADE OF BS1503
> -224 - GR.
> 28
>
>
>
> Dear Mr. Rohit,
>
>
>
> Thanks for the information. I have gone through it but it
> does not say
> specifically about224 - GR. 28
>
>
> Would you pl. thorw some more light on this.
>
>
>
> Regards,
>
>
>
> S.N.Dave
>
> --- On Tue, 8/5/08, Rohit Bafna <rohit@tcreng.com>
> wrote:
>
> From: Rohit Bafna <rohit@tcreng.com>
> Subject: [MW:994] RE: 993] EQUVIVALENT ASME GRADE OF
> BS1503 -224
> - GR. 28
> To: materials-welding@googlegroups.com
> Date: Tuesday, August 5, 2008, 9:05 PM
>
> Dear Mr. Dave,
>
> Please look at http://www.e-pipe.co.kr/eng/bs_no/bs_9.htm
> <http://www.e-pipe.co.kr/eng/bs_no/bs_9.htm>
>
> Regards,
>
> Rohit Bafna
>
> Director - Global Sales
>
>
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of
> shailesh dave
> Sent: Tuesday, August 05, 2008 8:39 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:993] EQUVIVALENT ASME GRADE OF BS1503 -224 -
> GR. 28
>
>
>
> DEAR MEMBERS,
>
> CAN ANYBODY LET ME KNOW THE EQUIVALENT ASME GRADE OF
> BS1503 -224-GR.28.
> WHERE FROM I CAN HAVE THIS INFORMATION AS READY RECKONER.
>
> REGARDS,
>
> SHAILEH
>
> QA/QC INCHARGE
>
> ADGAS DAS ISLAND UAE
>
>
>
>
>
>
>
>
>
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...