Skip to main content

[MW:763] Re: AET type exchanger test ring

Dear Jignesh ,
 
hope the attached file help you
 
good luck
Alireza

Jignesh Patel <nacemail@gmail.com> wrote:
Dear Friends,
 
I have seen few heat exchangers on this forum. I am an end user of heat exchangers in refinery. My query is related to test rings of exchangers.
 
One of our new units has AET type exchangers [pull through type]. These exchangers have a floating tubesheet [FTS] with bolt holes and the floating head cover [FHC] is directly bolted to the floating tubesheet. The problem with this is that we canâEURO(tm)t carry out shell test using a conventional test ring due to several bolt holes on the floating tubesheet. Conventional AES exchangers have backing rings pressing the FHC against the FTS.
 
I checked TEMA website and it says, test rings for such exchangers are possible and the bolt holes in the tubesheet need to be temporarily plugged. It also says refer to 4.13 (3) of TEMA. Unfortunately we donâEURO(tm)t have the latest edition of TEMA.
 
Does any one have experience with test rings [for shell test] for AET type exchangers? I would appreciate a generic drawing / scheme showing how to carry  out shell test of such exchangers.
 
Thanks in advance.
 
Thanks and regards,
 
Jignesh
Kuwait
 
For your virus protection, any attachments should be considered uncontrolled unless they are identified in the text. The sender does not accept liability for any virus introduced by this email or any attachment.
 


Be a better friend, newshound, and know-it-all with Yahoo! Mobile. Try it now. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Unknown said…
I am a fabricator, & have been asked to design the test ring for Heat exchangers, can anyone please help me in designing the test rings with regards to dimensions & MOC

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...