 Documents issued by the manufacturing plant

2.1 Certificate of compliance/Werkbescheinigung/Attestation de conformité Confirmation issued in text form without test results, confirming that the delivery corresponds to the agreement.

2.2 Test report/Werkzeugnis/Relevé de contrôle Confirmation based on results given for products made of the same/ similar materials, confirming that the delivery corresponds to the agreement.

2.3 Specific test report/Werksprüfzeugnis/Relevé de contrôle specifiqué Confirmation based on results of tests made on the delivery itself, confirming that the delivery corresponds to the agreement.

B3) Documents issued by experts independent of the manufacturing

3.1 A. Inspection certificate/Abnahmeprüfzeugnis/Certificat de réception Confirmation issued by an officially nominated inspector based on the results of tests made on the delivery itself according to legal rules, confirming that the delivery corresponds to the agreement.

3.1 B. Inspection certificate/Abnahmeprüfzeugnis/Certificat de réception Confirmation issued by the plant inspector based on the results of tests made on the delivery itself according to the requirements of the customer, confirming that the delivery corresponds to the agreement.

3.1 C. Inspection certificate/Abnahmeprüfzeugnis/Certificat de réception Confirmation is by an expert nominated by the customer based on the results of tests made on the delivery itself according to the requirements of the customer, confirming that the delivery corresponds to the agreement.



On Monday, October 5, 2009 at 1:49:51 PM UTC+3, ELAMARAN RAJAN wrote:
Dear Friends
 
As per our client specification for all welding consumables has to be minimum of EN10204 3.1 certification is required.
we are submitted EN10204 3.1 Chemical composition and for mechanical properties EN10204 2.2.
But Client not accepting that certificate due to mechanical properties has to be certified as per EN10204 3.1
 
let me know what is the difference between EN10204 3.1 and EN10204 2.2

regards
maran

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/90aec775-f43c-4c98-bbd7-a99edb5cf136%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...