Re: [MW:17461] WPS for A350 LF/2 forged flange

Yes, you can proceed with same WPS, as YS & TS are same for both.



On Thu, Apr 18, 2013 at 11:52 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
yes, you can


On Wed, Apr 17, 2013 at 7:10 PM, Ezat Adel <ezatadel2008@gmail.com> wrote:
Dear Expert ,

Could you give me your opinion about my supplier send me A350 LF/2 forged flange instead of A 105 N forged flange and i have a WPS for welding A 105 N to API 5l x42 in your opinion this wps will covered  A350 LF/2 to API 5l x42 ?

as i know  A350 LF/2 is a low temp.carbon steel and A 105 N is a carbon steel and both material has the same P no.,Group no. and in my activities i do not need to use a low temp. CS but my question  if i accept this flanges  the wps i have will covered the case.

the WPS i have is E6010 for root pass and E7018 for filling and cap

Thanks in advance

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--

Regards-

Jugesh Kumar- Manager-Projects, Velosi Certification Services (I) Pvt. Ltd.

E | jugesh@velosiindia.net , C | 9904426217/ 9547885665

T | +91-22-2164 9720  F | +91-22-2164 6392 W | www.velosi.com  
A | 505, 5th Floor, 360 Degree Business Park | Near Mulund Check Naka, LBS Marg | Mulund (West) | Mumbai - 400080 | Maharashtra | India |
                            
 
 
 Please don't print this e-mail unless you really need to.                               
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...