Hi Pradip,

 

Many thanks for all the info.  Agree 100% with you that one should not always stare at capital costs rather consider what the long term maintenance costs would be and always select the highest quality products especially for large projects but within the allowable budget. 

 

Regards,

 

Gerlof Oegema I PrTech Eng, BTech, BSc (Mech. Eng.)

Associate I Professional Engineering Technologist (Mechanical) I Aurecon

T +27 12 427 3140   I  M +27 82 805 4757

E Gerlof.Oegema@aurecongroup.com
Aurecon Centre, Lynwood Bridge Office Park, 4 Daventry St, Lynnwood Manor, 0081, Tshwane
I South Africa
aurecongroup.com


 

DISCLAIMER

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Tuesday, April 16, 2013 4:04 AM
To: materials-welding@googlegroups.com
Cc: Gerlof Oegema
Subject: RE: [MW:17417] Re: 17357] Austenitic Stainless steel piping, corrosion environment

 

Hi Gerlof,

 

Here're some foods for your thoughts. In tropical sea water environment  in North Africa, 304L would be highly unsuitable , 316L may last for some time (considering the facts that it contains 2.5% Mo to fight pitting corrosion). However Duplex and  Super Duplex or 6Mo alloys are long lasting and better engineered materials for such environments.

 

How does it matter with cost, e.g Duplex is more expensive than 316L? In a large project like power plant what percentage would involve  towards  cost of materials. Certainly build it right first time is a far better approach than "  let it fail and fix later".

 

The problem of power plant is that designers do not take corrosion as serious issue.  Whereas a materials and welding engineer in any oil and gas environments has to fight all the time.

 

The intent of my response is not educate others, but to emphasize  that  marine corrosion could be very aggressive and hence materials selection should be done accordingly.

 

Thanks.

 

 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Gerlof Oegema
Sent: Monday, April 15, 2013 9:38 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:17402] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

Hi All,

 

SS316L is normally regarded as "marine grade" but it all depends on the water quality and temperatures the 316L is exposed to.  SS316L is only subject to stress corrosion cracking (SCC) in the order and above 60 deg celcuis, which would result in crevice and pitting when exposed to warm water before even reaching the SCC phase.

 

Agree that super duplex is the better option but it all depends on the application that need to be investigated carefully and budget available as super duplex is double or more the cost of 316L.

 

Regards,

 

Gerlof.

 

 

 

DISCLAIMER

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Clubb, Archie
Sent: Monday, April 15, 2013 10:15 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:17389] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

 

Guys – Reading the mail trail and the responses:

 

SS 316L is unsuitable for an aggressive sea water application – Super Duplex is the option for undeaerated seawater and Duplex for Deaerated Seawater.

 

Archie

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shomenath Bagchi
Sent: 14 April 2013 05:58
To:
materials-welding@googlegroups.com
Subject: Re: [MW:17373] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

 

SS 316 L is used in marine environment and is better suited.

 

 


From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: pgoswami <
pgoswami@quickclic.net>
Cc: "
materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Saturday, April 13, 2013 12:42 PM
Subject: [MW:17368] Re: 17357] Austinitic Stainless steel piping, corrosion environnement

 

Dear sir,

   it will be for power plant, especially for facilities in front of water sea.

Regards.

 

2013/4/13 pgoswami <pgoswami@quickclic.net>

Where you want use these pipes?

 

Would it be for power plant application or for design and construction of any oil and gas plant ?

 

Please elaborate.

 

Thanks

 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Friday, April 12, 2013 12:23 PM
To:
materials-welding@googlegroups.com
Subject: [MW:17357] Austinitic Stainless steel piping, corrosion environnement


Dear experts,

  Need your help.

Need to confirm if we can use austinitic stainless steel piping (A312 304L & 316L grades)  for maritime environnent and any risk of corrosion.

To code/standard i can refer ?

Regards.

-----

زكرياء غراب
GHRAB Zakaria

Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/groups/opt_out.
 
 




--

زكرياء غراب
GHRAB Zakaria

Jorf Lasfar Units 5&6 Power Plant construction Project
EA2C/ SDEM Entreprises
Site QA/QC Manager
Mobile : Morocco (+212) 6 61 07 00 11
             Tunisia (+216) 96 635 805



Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/groups/opt_out.
 
 

 

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/groups/opt_out.
 
 

 
*************************************************************************
This e-mail message and any attachments to it are intended only for the 
named recipients and may contain confidential information. If you are not
one of the intended recipients, please do not duplicate or forward this
e-mail message and immediately delete it from your computer. If you 
received this email in error, please notify postmaster@veoliawater.com
*************************************************************************
 
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...