Dear Mr. Pundir,
 
I suggest you to keep holding period 30 Minutes considering 10 mm. Nom. Thk. Following vendors can do the job successfully.
 
(1) Ratnamani Heating Point, Odhav, Ahmedabad- Contact No. 079-22974313.
 
(2) Heat treaters & Engineers- Ankleshwar- Contact No. TELFAX NO 02646-221190.
 
(3) Gujrat Perfect Engg. Ltd., Vadodara- 9898014997.
 
Thanks & regards,
 
C. R. GANDHI


--- On Fri, 4/12/13, A. K. Pundir <pundir@milindia.in> wrote:

From: A. K. Pundir <pundir@milindia.in>
Subject: [MW:17353] Quenched annealing of SS 116 Vessel
To: materials-welding@googlegroups.com
Date: Friday, April 12, 2013, 11:31 AM

Dear All,
 
Need your suggestions on PWHT(Quenched annealing) of SS 116 Vessel with following details.

 

1.T.L to T.L=1590mm

2.Totel length=2165mm

3.Shell Dia=1168mm

4.Thickness=10mm

5.Material A240 TP 316L,A312 TP 316,A182 TP 316.

6.Soaking Temperature-1950 ̊F

7.Soaking Time- 105 minutes

8.Rate of Cooling-water Quenching

 

If this Heat Treatment is possible please suggest the good Heat Treatment shop in India.

 

Regards

 

A.K.Pundir

Dy. Manager(Q.A)

MILINDIA LTD.,

W-31, SECTOR-11,

NOIDA - 201 301 (U.P)

09871607731

  ** Message has been scanned by Emergic MailServ **
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...