Dear Experts, We are going to qualify welding procedure of following details 1. Welding with · GTAW with ER70S2 · SMAW with E7018-1 & · SAW 2. Heat treatment after welding at 620°C @ 200min 3. Impact testing after heat treatment at -46°C Kindly advise on filler metal & Flux combination for SAW process to achieve impact properties after heat treatment. Can F7A8 EM12K will this serve the purpose…!! Thanks & regards Ali Mhaskar, | ||
|
Wednesday, April 10, 2013
[MW:17336] Request to provide filler metal & Flux combination for SAW process for low temperature service with Heat treatment
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...