Friday, February 15, 2013

[MW:16773] Re: P1 MATERIAL TO 2205 MATERIAL

Dear ,

You can use E2209 rutile coted electrode, remember colling rate after welding shall be low.

regards,
Vineet Kumar
9971055188


On Friday, February 15, 2013 9:25:34 AM UTC+5:30, Bala Nechur wrote:

HELLO EXPERTS,

 

i HAVE SOME WELDING 2205 DUPLEX MATERIAL TO P1 GROUP,  FILLET WELD.  PLEASE SUGGEST RECOMMENDED ELECTRODE.

 

BALA

780 204 0239

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...