Dear Amit Vishwakarma
AS PER ASNT-TC-1A THE NDT PERSONAL MUST QUALIFY EYE TEST
8.2 (2) Contrast Differentiation. The exami-
nation should demonstrate the capability of
distinguishing and differentiating contrast
among colors used in the method. This
should be conducted upon initial certifica-
tion and at three-year intervals thereafter.
BEST REGARDS
N.SELVANESAN
On 9/7/12, VishwakAmit <amitspvishwak@gmail.com> wrote:
> Dear Experts
>
> I have strange doubt that whether color blindness person can do NDT
> inspection or not but person practically facing no problem and
> is it Mandatory requirement that NDT inspection shall be normal vision
> person,,,,?
> if Yes, then what extent he can do NDT inspection
>
> Regards
> Amit Vishwakarma
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
N.SELVANESAN
00971557112613
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...