dear sir
i think you need tpo keep post heaqt 150- 200 c
and you shold keep inter pass temp 250-300 c
regards
On 8/23/12, suresh <sureshndb@gmail.com> wrote:
> Dear Members,
> we found some weld cracks on parent metal (adjacent to weld bead)
> after weeding and depth of the crack is max 20 mm from the edge of the
> plate.
> i would like to know the type of crack and causes of the crack.
> please see the attached pictures.
>
> Material:- IS 2062 Gr B to Itself
> Thickness:- 25mm to 25mm
> Joint Type:- Closed Corner
> Grove Type:-Single side bevel
> Electrodes:- E 7018
> Preheating:- 80 to 100 Deg Cent
> Electrodes Baking:- As per manufacturer recommendations.
> waiting for your valuable reply.
>
> Thanks and Regards,
> Suresh,
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment