Re: [MW:15193] Impact Test clarification

Make a supplementrary coupon with same welding parameters and do impact test. at -46 deg.C and attach with the original PQR.

Thanks & Regards
Muhammed Ibrahim PK



On 3 September 2012 05:33, mubeen mubeen <mubeenaws@gmail.com> wrote:
Dear experts, 

Please help out to clear my doubt. 

I have qualified a WPS/PQR with impact -29 deg C, now customer want the WPS/PQR shall be qualified with impact in -46 deg C. Also there is no remaining coupon piece available for impact testing with -46 deg C. 

My question here is, should I weld a coupon and only do impact test as required by customer and attached to PQR will be sort out this issue.? 
or 
Should I REDO a PQR with all mechanical  test which includes Tensile, Hardness, Bend along with impact will sort our this issue.? 


Requesting you to please provide me ASME IX clause reference.


Anticipating for you kind help. 

Thanks & Regards. 
M.K.Mubeen

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...