Dear Experts,
As per ASME Section VIII Div I.
UW-51, RADIOGRAPHIC EXAMINATION OF WELDED JOINTS
t = the thickness of the weld excluding any allowable reinforcement. For a butt weld joining two members having different thicknesses at the weld, t is the thinner of these two thicknesses.
As per ASME Section I
PW-51 RADIOGRAPHIC EXAMINATION
t is the thickness of the weld
My question is As per ASME Section I, whether t is the thickness of the weld including or excluding any allowable reinforcement ?
Regards
Hiren Sevak
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment