Samshuddin,
This depends on the type/grade of material you are working with. Some
material require RT as soon as the weld cools, some material 24hrs after
welding, some 48hrs, while some 72hrs after welding. It all depends on
your material.
Note: some material demand NDE before and after PWHT
"Quality is the Bone, Be the Dog Always"
Boniface Obidike
QA/QC Engineer
Speciality Connectors & Pipes
Drilling and Production Systems
GE Oil & Gas Business
Mail: Boniface.Obidike@ge.com
Office: +234(1)4629400
Mobile: +2348163479738
Home: +2348039409934
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of samshuddin k
Sent: Thursday, May 03, 2012 4:03 PM
To: materials-welding
Subject: [MW:14178] Fwd: Time span for RT after PWHT
Dear Sir
Good Evening
Generally after 72hrs of welding, we will do RT.
But in our repair marine project, we dont get sufficient time to follow
this.
Is it acceptable by Code (ASME /AWS) to do RT immediately after PWHT
Please guide me with Code reference.
regards
Samshudddin.K
NKOM Qatar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
This depends on the type/grade of material you are working with. Some
material require RT as soon as the weld cools, some material 24hrs after
welding, some 48hrs, while some 72hrs after welding. It all depends on
your material.
Note: some material demand NDE before and after PWHT
"Quality is the Bone, Be the Dog Always"
Boniface Obidike
QA/QC Engineer
Speciality Connectors & Pipes
Drilling and Production Systems
GE Oil & Gas Business
Mail: Boniface.Obidike@ge.com
Office: +234(1)4629400
Mobile: +2348163479738
Home: +2348039409934
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of samshuddin k
Sent: Thursday, May 03, 2012 4:03 PM
To: materials-welding
Subject: [MW:14178] Fwd: Time span for RT after PWHT
Dear Sir
Good Evening
Generally after 72hrs of welding, we will do RT.
But in our repair marine project, we dont get sufficient time to follow
this.
Is it acceptable by Code (ASME /AWS) to do RT immediately after PWHT
Please guide me with Code reference.
regards
Samshudddin.K
NKOM Qatar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments