Wednesday, June 2, 2010

RE: [MW:5354] Hardness requirement for P1 material

What is your code of construction?
For e.g. If it is B31.3, refer PWHT table. Else if NACE is applicable, refer NACE std also.
Sent from my Nokia phone
-----Original Message-----
From: Dharmesh Mistry
Sent: 02/06/2010 1:56:10 pm
Subject: [MW:5351] Hardness requirement for P1 material

Dear all,

Please let me know where I can find hardness requirement for P1
materials.

Thanks & Regards,

DHARMESH MISTRY

Direct : +91 22 6774 0074

Cell +91 98207 35814

Dharmesh.Mistry@heurtey.in

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...