Thursday, November 12, 2009

[MW:3636] About HARDNESS

DEAR FRINEDS,

Can you please let me know which section(asme b 31.3) mentioned the
hardness value for cabon steel(A106) and Low temp material (A 333)

thank you
ranjith

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

Suresh Paidi said...

It should not be exceeds 225 BHN .

Suresh
Fluor

[MW:34916] Applicability of Impact requirement as per ASME B31.3