Re: [MW:35529] IMPACT ASME SEC IX WPS/WQT

WPS/PQR for Mechanical properties & Welding Performance Qualification for Welders is to verify his ability to make sound weld. Impact does not have any influences on welder performance.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Apr 7, 2025 at 1:32 PM Elavarasan Mech <elavarasan1861994@gmail.com> wrote:
Dear Expert     
 we have qualified WPS for 8 mm  & 25 mm plate with impact (8-16 mm  range & 16-50 mm ) as per ASME sec IX 
What about the welder qualifications we need to be consider impact requirement same as per WPS or impact requirements doesn't required for welder qualifications please guide me

Regards 
ELAVARASAN 

   



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yma_rkksaAF0azyoL7jbiNNjZrp3taCiuHHWdumPT5mMg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP8rLHYtQfOLMAzE_4-Dk_AiYXyaPehiHZSYp3ukM%3DJJQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...