Re: [MW:35506] WPS for Furnace PWHT

Dear Sir,

I am not clear about the question.

Is the question is "The welding is done without following a WPS having  PWHT and actually the joints need the same" is it?

May I know the material ?

Also if it is of Carbon Steel material, is PWHT requirment is there based on design or based on ASME 31.3?

Regards,

Hareesh K V

On Mon, 27 Jan, 2025, 11:57 am Prakash Kumar Bontra, <prakashbontra@gmail.com> wrote:
For furnace PWHT as per ASME B 31.3 all the joints in the spool (1" to 36") need PWHT approved WPS and where to refer?

Prakash Bontra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANeLWoNy0URXS9X7TEvvZRVe4V-1LNPKwidHJ097fDyPAjyh7Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEv1fk_qTuLX3BbXwWEmjZYkHEKJg5fYEQ4n3tV28CtXxXG8DA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...