Monday, April 7, 2025

[MW:35523] IMPACT ASME SEC IX WPS/WQT

Dear Expert     
 we have qualified WPS for 8 mm  & 25 mm plate with impact (8-16 mm  range & 16-50 mm ) as per ASME sec IX 
What about the welder qualifications we need to be consider impact requirement same as per WPS or impact requirements doesn't required for welder qualifications please guide me

Regards 
ELAVARASAN 

   



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yma_rkksaAF0azyoL7jbiNNjZrp3taCiuHHWdumPT5mMg%40mail.gmail.com.