Re: [MW:33370] USER's definition in API codes

Dear Krishna, 

In your case you must use epoxy grouts in all cases, 
And the Client/User/Owner can say whether the use epoxy grouts for all machinery can have any other alternative method or not. 
EPC dont have the right to override this. You may also raise a TQ to get a waiver or any alternative ways for this from client.

regards



On Monday, 8 August 2022 at 03:19:14 pm SGT, 'JOEL REMOROZA' via Materials & Welding <materials-welding@googlegroups.com> wrote:



Inline image


On Monday, August 8, 2022 at 10:03:21 AM GMT+3, Raghuram Bathula <raghurambathula@gmail.com> wrote:


see definition 2.20

On Mon, 8 Aug 2022 at 12:26, krishna kamal nayan Pandey <kkmech1987@gmail.com> wrote:
Dear Experts,
We have some ongoing arguments at site with reference to the word "USER" in API 686.

"Unless otherwise specified by the User, all machinery shall be grouted using epoxy grouts."

With the above statement in API 686 , User is defined for EPC contractor or Client / Owner.

Please advise.

Best Regards,

 

Krishna Kamal Nayan  



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CADxVub%3DeYeoWHc_OFitnbWBqc8N8ikBJOq5iFq5A_uR2y2VkKA%40mail.gmail.com
.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/132527853.1157107.1659942536354%40mail.yahoo.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...