Hi!
I think multiplying factor for smaw seams low we used to take 1.5 to 1.7 × Theoretical wt of joint


On Mon, 1 Aug 2022 at 15:30, srinivas rao
<engr.srini@gmail.com> wrote:

Hi Sachin ,                                                                                     

 In addition to trailing mail formulas, you can also approach with different ways for calculating / arriving formulas for the weight with reference to groove designs involved in drawings.

weight of weld metal for each joint should be multiplied by the some wastage factors  to arrive final weight of welding consumable required for joint.

These factors are achieved based on some assumptions like minimum wastage, optimized practices for utilization of electrodes/filler wires, minimised unnecessary scraping by maintaining good engineering practices of consumable handling etc..

Refer below multiplication factors for common welding processes used at site /shop work places.

Arc welding process               Multiplication factor

GTAW                                           1.1 to 1.15

SMAW                                          1.5 to 1.8

GMAW                                         1.05 to 1.1

SMAW                                          1.05 to 1.1

FCAW                                             1.1 to 1.2

At initial stages of work, you can go with above calculations and during production welding progress the Actual multiplication factors can be derived for your application by observing the actual consumption during the production welding of each size/joint type at your factory /or site work. And re-do theconsolidate the consuamble quantity for final purchase. 


Thanks& Regards,
Srinivas Rao
welding Engineer
On Sunday, July 31, 2022 at 11:45:06 AM UTC+4 Sham Shahabuddin T I wrote:
Dear Mr. Sachin 

Please find the attached for consumable weight calculation slides.

Regards
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING



On Sat, Jul 30, 2022 at 5:00 PM Sachin Gonjare <sachins...@gmail.com> wrote:
Dear All Experts
Please help me ,I want to do actual costing (for arc and CO2 welding)of gas consumption,electrode consumption,CO2 wire consumption.If have any data please share. .
Regards
Sachin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/41fff519-0578-4a14-aa9b-1b74a2733c45n%40googlegroups.com
.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/388433705.3811156.1659348609489%40mail.yahoo.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...