Hi Ankit,
You have to design-perform mock up as per IBR.
IBR inspector will also witness the TTS Mock up welding and lab test.
On Fri, 4 Sep 2020, 5:02 pm Patel Ankit, <aapatel271@gmail.com> wrote:
Dear Expect,--Currently I have one IBR job in my project.Equipment is HP Heater.In this job I have do tube to Tubsheet Strength welding.Pl suggest any additional test for This TTJ joint.Sir can you tell me about this?Regards,Ankit Patel
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuxNibPVGrdhGhoqZYaE%3DU3UUa5BBGB8JKEgNKui_grNQA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM94n3qaArdKgCn4gLzVcg%3D38Km9qvkZd5nnahRwaDaVD851og%40mail.gmail.com.
No comments:
Post a Comment