only difference is impact test temprature.

On Wed, 2 Sep 2020, 10:00 am Ghulam Mustafa, <gmt.lah@gmail.com> wrote:
Dear All,
Hope you are fine.
i want discuss that i was gone yesterday for inspection in other company as a third party, i checked WPS for welding inspection, during inspection i observed that welder used E7018-1 Electrode instead of E7018 on structure. structure material A572 Grade-B and A-36. E7018-1 can problem or not?
can any one tell me about this problem.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b55e87f5-633e-477c-b7ad-be9aa33fcd52n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k_cizXsTwn9KsiK0z8a8tNQWC0zs6jFO%2BvUifaKnq-TJw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...