Re: [MW:31382] E-7018-1 is better then E7018

The difference between E 7018 and 7018-1 is the impact test temperature, so 7018-1 is better than 7018

في الأربعاء، ٢ سبتمبر، ٢٠٢٠ ٨:١٤ ص yomna Ahmed <ahmedelsayedhd2015@gmail.com> كتب:
No proplems

في الأربعاء، ٢ سبتمبر، ٢٠٢٠ ٨:٠٠ ص Ghulam Mustafa <gmt.lah@gmail.com> كتب:
Dear All,
Hope you are fine.
i want discuss that i was gone yesterday for inspection in other company as a third party, i checked WPS for welding inspection, during inspection i observed that welder used E7018-1 Electrode instead of E7018 on structure. structure material A572 Grade-B and A-36. E7018-1 can problem or not?
can any one tell me about this problem.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b55e87f5-633e-477c-b7ad-be9aa33fcd52n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKvnTKqhX8CLxy3sO-ic4MaN48Uk%2BmMedtougV8p2eUenrRKfw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKujbmtPGTJ28MMSuyxUKkX4h2q2ie00WWfcRR5qMcoN-wynbA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...