On the internet you can find tables where they suggest contribution materials, generally these tables are based on the experience of other people in the area.
This table was shared with me in this group.
Regards!.
Regards!.
El mar., 7 jul. 2020 a las 0:29, vinu raveendran (<vinuravi007@gmail.com>) escribió:
Dear Suresh,--Refer API 577, Annexure D for selection of consumables with base metal
On Monday, July 6, 2020 at 8:05:41 AM UTC+3, SURESH KUMAR TS wrote:Dear All,Please can you suggest how to choose the filler material for the different material,what are all the basic things we need to know:if you guide and share with an example what you are followingit will be of great help.Any app your using for searching the filler rod, dear all please share your thoughts on this topic will be great help to other as well.Thanks in AdvanceSuresh Kumar TS
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f42a2164-54c0-436a-ab81-b6e533f4fe1fo%40googlegroups.com.
Ing. José Juan Jiménez Alejandro
Independent Consultant in Parts
and Pressure Equipment
SSI-TPI
Móvil +52 1 812 352 4606
Skype: jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLtWb2UB4ay%2Bcx2rprR-j99hvh8c-v6T1f5kPgR9U86SQ%40mail.gmail.com.
No comments:
Post a Comment