Both are same P.no8/Group.no1.
So no issue to use the old WPS.
But must be consider,
1. Special requirements other essential variables such as thickness range,
And supplimentry essential variables,
Based on particular project requirements.
2. Approval of new client.
என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584
Thanks & Regards,
RAJAVARMAN
+971561895584
On Tue, Jul 7, 2020, 9:29 AM Dharma dattu <dharmadattu@gmail.com> wrote:
Hello All,--We have a new project for which main components are SA 312 TP 304L material, currently we have SA 312 TP 304 WPS can we ues the same, as the Pno. is same!Regards,Dharma Dattu. B
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/89ae66ad-2aad-40ce-aed3-fe009c801617o%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU5x7ZBveDnvsZ3eAf07ihUDEs0ty_MXqGD0Ypbtg0%3DEQw%40mail.gmail.com.
No comments:
Post a Comment