Monday, July 6, 2020

Re: [MW:31105] HOW TO CHOOSE WELDING ROD FOR DIFFERENT MATERIALS

Dear Sir, 

Thank you for the response.

lets go in detail , i will quote a example, to start with, i need to weld from material SS-304 to material SS-304,

what are all the consideration we need to look in to, 
As you suggested first we need start from material mechanical and chemical properties.
presently what are the ways you recommend, is there a common pool (like website or any specific recommendation of material brand website for referring data sheet) for checking the details or we just google it any random results can be used. 
if you could suggest ... any books & website that we can refer for mention any material we can get the mechanical and chemical properties. 

screen shot of material properties 




Thanks & Regards
Suresh Kumar TS
+91-9535256508

On Monday, July 6, 2020 at 10:53:41 AM UTC+5:30 Rajavarman wrote:
To choose filler rod,

Make a table of
Chemical and mechanical properties...
Try to find the highest grade materials,

Choose the electrode properties which next higher level than parent meterials.

Also, consider the another materials property also.

Normally online website are aavailable to choose the electrode.
Try that also

என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Mon, Jul 6, 2020, 9:05 AM SURESH KUMAR TS <sureshku...@gmail.com> wrote:
Dear All,

Please can you suggest how to choose the filler material for the different material,

what are all the basic things we need to know: 
if you guide and share with an example what you are following 
it will be of great help.  

Any app your using for searching the filler rod, dear all please share your thoughts on this topic will be great help to other as well. 

Thanks in Advance 
Suresh Kumar TS



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c66ec19c-59a1-4543-b90a-c7e3704a1b86n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/21080cd9-182c-4877-9521-84cbd72c4b0cn%40googlegroups.com.

No comments:

Re: [MW:35507] WPS for Furnace PWHT

As per ASME B31.3, Clause 331.1.6 (b): Any required PWHT shall be carried out in accordance with the qualified WPS. For furnace PWHT inv...