Monday, July 6, 2020

Re: [MW:31104] HOW TO CHOOSE WELDING ROD FOR DIFFERENT MATERIALS

To choose filler rod,

Make a table of
Chemical and mechanical properties...
Try to find the highest grade materials,

Choose the electrode properties which next higher level than parent meterials.

Also, consider the another materials property also.

Normally online website are aavailable to choose the electrode.
Try that also

என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

On Mon, Jul 6, 2020, 9:05 AM SURESH KUMAR TS <sureshkumar.dfab@gmail.com> wrote:
Dear All,

Please can you suggest how to choose the filler material for the different material,

what are all the basic things we need to know: 
if you guide and share with an example what you are following 
it will be of great help.  

Any app your using for searching the filler rod, dear all please share your thoughts on this topic will be great help to other as well. 

Thanks in Advance 
Suresh Kumar TS



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c66ec19c-59a1-4543-b90a-c7e3704a1b86n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BHpzU5KtYXNtPpvpSrUmS5Dq2sueWuBvp7qHOUb1rhM400xDg%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...