Wednesday, July 8, 2020

[MW:31121] Suitability for wps

Hi friends

I have made a wps in 3g as per AWS d1.1 , I was under the impression that if I qualify in 3g it will automatically be qualified for flat and horizontal.But it seems there is a code restriction for this and I can weld only 3g for production welds.
My doubt is if i make one more test coupon in 2g for the same wps and get it qualified will it work??
Or should I need to create a new wps jus for this 2g position ??

Thanks in advance
Chris

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20faa944-10b0-405c-9707-39f286836ff5o%40googlegroups.com.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...