[MW:31111] Re: HOW TO CHOOSE WELDING ROD FOR DIFFERENT MATERIALS

Dear Suresh,

Refer API 577, Annexure D for selection of consumables with base metal

On Monday, July 6, 2020 at 8:05:41 AM UTC+3, SURESH KUMAR TS wrote:
Dear All,

Please can you suggest how to choose the filler material for the different material,

what are all the basic things we need to know: 
if you guide and share with an example what you are following 
it will be of great help.  

Any app your using for searching the filler rod, dear all please share your thoughts on this topic will be great help to other as well. 

Thanks in Advance 
Suresh Kumar TS



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f42a2164-54c0-436a-ab81-b6e533f4fe1fo%40googlegroups.com.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...