Application ??
On Sat, 2 May 2020 at 13:55, Baha <b.nikrooz@gmail.com> wrote:
Hi--Is it acceptable to use plate instead of cladding for blind flange? The cladding material and plate is CU NI 90/10.The below drawing is the manufacturing offer.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3612b777-edba-433e-8658-cf93bc126f3d%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oi9XAv33ABcNk7D8VPiWvpyyiOH-bYgW-Qt8VERw1VWMA%40mail.gmail.com.
Comments