Dear Experts
Kindly please put your valuable points, that where is the soaking time mentioned in the ASTM A182 standard materials. I can see only heat treating requirements like temperature,cooling media, quenching cool etc. 

Note: Can i take per inch, 1 hr soaking time

Regards
Suresh kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fde80f50-bcd1-4f42-8d38-c08eb2f7adb7%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...