What are the guidelines for selection of Soultion A/B/C when using NACE TM0284 7 0177?
Regards
Chandu

On Mon, Apr 13, 2020 at 9:50 AM TDK YOKESH <tdky167@gmail.com> wrote:
Dear sir,
Kindly see the requirements specified in Nace MR0175 clause 8. 


On Mon, Apr 13, 2020, 7:46 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
1. Final Heat Treatment condition
2. If Repaired, Qualification of PQR with Hardness requirements & Locations
3. Base Metal Hardness requirements
4. Chemical composition restriction like sulphur and Nickel
5. Based on Purchaser requirement, any HIC or SSC test

Thanks & Regards

J.Gerald Jayakumar



On Sunday, April 12, 2020, 11:20:27 AM GMT+7, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear friends,

if we place the order to any steel foundry to supply the casting ( A 216-WCB)  with NACE requirements. while see the casting MTC they use to mention the above casting are meeting the requirements of NACE MR 0175 or MR 0103 requirements
means what? what are the additional activities being followed for NACE castings in foundry than standard casting ? can you any body give me a details.   

Regards,
Sankaran.SP
Welding & Metallurgy expert

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1625659408.2218431.1586593902186%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/679013541.2894413.1586673439058%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuoZPU4mYgWX%3DrBq66jm4dzMirBN6r6t7JEOpyyvt7DHHQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKjKdNYPoGftVnUXHm0gVdNNRV_hXbGaLv%3Der327eOqtnnaMTg%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...