Friday, May 22, 2020

Re: [MW:30906] Heat treatment requirement for SS310 vs SS347

No need 


Sent from Yahoo Mail for iPhone

On Friday, May 22, 2020, 10:53 PM, Arun Nair <arunnair.mundakkal@gmail.com> wrote:

Hello,
 Weld joint between SS310  to SS347 kindly advice about heat treatment require or not? Either pre or post.

ArunNair

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM8%3Dvxqa%2BZJyP4_idWdODyDJCK27L2VO1EPvGdgqtbN%2Bikxqdw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...