Monday, May 11, 2020

Re: [MW:30861] Radiography can be done After Hydrotest

As per ASME B 31.3 ,clause 345  "Prior to initial operation, and after completion of the applicable examinations required by para. 341, each piping system shall be tested to ensure tightness. The test
shall be a hydrostatic leak test in accordance with para. 345.4 except as provided herein."
Here clause 341 calls for NDT and Visual examination. 
Hope its clear now that hydrotest shall be after NDT but if client accepts than sequence can be reversed.

Thanks and regards
Atul Khatri

On Sat, May 9, 2020 at 11:07 AM 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Yes, you can do. provided your graphs should have within limited indications as per acceptance table. 
In case any one weld goes repair hydro test shall be done. 
Regards, 
S.SENTHILKUMAR 


On Sat, 9 May 2020 at 6:12, pradip kumar Sil
Dear All,
 Radiography  can be done after Hydrotest. What's the limitation of  ASME B-31.3.
Before Hydrotest all Radiography can be completed. ASME -B-31.3 Code reference ?
Your advice is highly appreciated with code reference ASME B-31.3.
Regards,
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DwM9yo%2B%3DLuNU3J185gWHOmY5DHvxnpvLz_uF3BVnjkUg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1568662456.343936.1589002308836%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeAV6m2OdDDdTsA06FvpuWas9_Nrf34waGrxwvAcNSkhjw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...