At least a dozen chromium molybdenum (CrMo) steel combinations exist. One of the more recent alloys consists of chromium, molybdenum, vanadium, niobium (columbium), and nitrogen. This material became popular for use in high-temperature applications, such as gas and coal-fired power plants. However, it is not intended to replace other CrMo types. Each alloy has its own place in the high-strength, low-alloy group of materials.

On Friday, 29 May 2020 09:52:44 UTC+3, tamizh wrote:
Dear Experts

can anybody answer for the below questions.?

What special processes are required on Cr alloy material welding?


 
With Warm Regards,

S.TAMIZH SELVAN,

          

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/98a3bccd-abb7-4adb-bbf1-4259471627f6%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...