Re: [MW:30854] Radiography can be done After Hydrotest

Yes, you can do. provided your graphs should have within limited indications as per acceptance table. 
In case any one weld goes repair hydro test shall be done. 
Regards, 
S.SENTHILKUMAR 


On Sat, 9 May 2020 at 6:12, pradip kumar Sil
<pradipsil@gmail.com> wrote:
Dear All,
 Radiography  can be done after Hydrotest. What's the limitation of  ASME B-31.3.
Before Hydrotest all Radiography can be completed. ASME -B-31.3 Code reference ?
Your advice is highly appreciated with code reference ASME B-31.3.
Regards,
Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DwM9yo%2B%3DLuNU3J185gWHOmY5DHvxnpvLz_uF3BVnjkUg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1568662456.343936.1589002308836%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...