Thursday, May 14, 2020

[MW:30874] Welding of DissimilThickness

Team i want to know how it can be possible to weld materials with dissimilar wall thickness of 5mm. DSS pipes to flanges. Flanges are higher than the pipes in thickness with 5mm.

--