Dear Charles,

The choice of welding parameters like current and Voltage is dependent on the choice of welding process and consumable used and not on Carbon Equivalent. Carbon equivalent is a weldability factor which gives you sense of materials conditioning prior to welding like preheat temperature and during welding and after welding for the avoidance of welding issues like cracking.

Regards
Rems


On Wed, 27 May 2020 at 16:22, charles
<charlesvj@gmail.com> wrote:
Dear experts,

Pl. Provide the calculation for finding welding parameters like current and voltage if the carbon equivalent of steel is known?. Does this work good for alloy steels also?

Regards,

Charles Jacob

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ac50252a-08b6-44f2-befe-638f83d70dbd%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1864823081.1082586.1590680441600%40mail.yahoo.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...