[MW:30869] Reference Thickness

Hi Gents,
We have a partial penetration (S=21mm)  with  5 mm leg length joint configuration ; (Tee Joint - combination weld (partial pen + fillet weld)
As per Client requirements if reference thickness is more than 25mm NDT should performed after 48 hours. (Reference thickness is

Could you please advise in our case what is the reference thickess 21 or 26 mm (21mm+5mm)



Regards,
Ilkin Hasanov.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYx_%3DoAOWk_S4Swb7CzdC9zWF%3DTEHEbhorJzb8QiZG6Hg%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...