Thursday, May 14, 2020

Re: [MW:30871] Reference Thickness

Dear  Ilkin,

 If the "leg size" is 5mm then the throat is 3.5mm and you end up with 21+3.5=24.5 mm
In these calculations the throat of the fillet weld should be taken into consideration and not the leg size.

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Wed, May 13, 2020 at 3:31 PM Ilkin Hasanov <ilkinhasanov.91@gmail.com> wrote:
Hi Gents,
We have a partial penetration (S=21mm)  with  5 mm leg length joint configuration ; (Tee Joint - combination weld (partial pen + fillet weld)
As per Client requirements if reference thickness is more than 25mm NDT should performed after 48 hours. (Reference thickness is

Could you please advise in our case what is the reference thickess 21 or 26 mm (21mm+5mm)



Regards,
Ilkin Hasanov.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYx_%3DoAOWk_S4Swb7CzdC9zWF%3DTEHEbhorJzb8QiZG6Hg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUjmasXhOT3eXhwrUh0rmZrSOVUMtmzcN4sOdAwY%3Dm7mZw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...