Friday, May 15, 2020

[MW:30875] Welding Travel Speed

Hello,

I need to do some calculation with weld parts and normally i use standard parameters for the calculation of the travel speed.

My problem it's to find tables with these reference values for the weld of plate of 20-30mm of tickness.
Normally for small tickness i use about 30dcm/min the travel speed value.

Can anyone welp me?


thanks

--