Re: [MW:30882] CLARIFICATION ON PQR DATE

Dear,
WQT date is 10/10/2019 and PQR date is 24/11/2019 is correct.

On Fri, 15 May 2020 at 8:34 PM, <sathishmech04@gmail.com> wrote:
Dear Experts
Kindly clarify below doubt's
Standard: ASME Sec IX

I have conducted procedure qualifications(welding done with recording all parameters) on 10/10/2019 and mechanical testing where conducted on 24/11/2019 in that all the testing were cleared. So my doubt is what date need to be endorsed that is during PQR generated test date or after mechanical test conducted date.

Kindly confirm


Regards.satti

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ae78523-7f75-457f-8941-d8289a5e4d84%40googlegroups.com.
--
Regards
CHANDAN SINGH
Sterling & Wilson 
+919981575817
+917379619175


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BtZUbVQmNMJmT%2BgARFvY-xOQsRSqOa2qCExs7MOjt94548Z1Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...