Dear experts,
I recently received one TQ for RTR pipe usage 2 inch and above. But in our project we need to use 1inch RTR pipe for the drain purpose.
My question is is that use 1 inch dia RTR pipes?
Please advise
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/479ff8e0-3e69-4623-9f4c-a66488e9c4c8%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
[MW:35633] IP Joint
Hello experts, I would like to know what is IP joints in piping(31.3)? Regards Saurabh -- https://materials-welding.blogspot.com/...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...