Dear Expert need your opinion.

I have WPS/PQR of dissimilar metal GTAW (F11 to SS316L) with Inconel Filler for high temperature application. Inconel filler selected according to API 582 guidelines..but our end user is not accepting Inconel filler because it doesn't have Moly content which is present in base metal.

Any document or write to prove correctness of Inconel filler?

On Tuesday, September 20, 2016 at 11:12:09 AM UTC+5:30, vijay Katkar wrote:
Dear Expert,

Need your guidance,

I have PQR with P1 to P43 with 10 mm thickness,

Can i use this PQR for Joint with 10 mm (P1) & 45 mm (P43) under following clause?

Clause no QW 202.4.



Thank you 

Vijay Katkar   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1db890c8-5cc2-4bae-b53a-ab54a0ee014e%40googlegroups.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza






Libre de virus. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurL0M04YhzyNneKB5FK%3DwfU%3DiqHYdR2FaX04vvtSbK9KNA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...